This table contains time-resolved rheometry measurements of a cyclo-aliphatic polyamide melt at 270°C under an oxidative dry air environment. Each row represents a measurement step recording viscoelastic properties, including storage and loss moduli and complex viscosity, over a period of two hours. The data tracks the influence of edge oxidation on the polymer melt's structural changes.
This table is useful for studying the kinetics of thermo-oxidative degradation and the resulting changes in viscoelasticity of polyamides. It provides raw experimental data for modeling edge gelation effects. It does not contain data for nitrogen environments or other temperatures (260°C or 275°C).
760 rows · 9 columns · published by Materials Cloud · licence: Open use, source must be named
Source file: https://archive.materialscloud.org/api/records/y12y2-j2z84/files/TPA_270C_Dry_Air_10rad.c… · the dataset
| Column | Type | Description |
|---|---|---|
| Step Time | FLOAT | The time elapsed since the start of the measurement step. |
| Oscillation Strain | FLOAT | The applied strain amplitude during oscillation. |
| Oscillation Stress | FLOAT | The measured stress response during oscillation. |
| Tan Delta | FLOAT | The ratio of loss modulus to storage modulus. |
| Storage Modulus | FLOAT | The measure of elastic energy stored in the material. |
| Loss Modulus | FLOAT | The measure of energy dissipated as heat. |
| Complex Viscosity | FLOAT | The overall resistance of the melt to flow. |
| Oscillation Torque | FLOAT | The torque measured during the oscillation cycle. |
| Gap | FLOAT | The distance between the parallel plates of the rheometer. |
Query it in SQL · API · Use it from an AI agent (MCP) · More tables
Cleaned and typed by Data Cleaner: open this file in Data Cleaner or clean your own file.