Rheometry of Cyclo-aliphatic Polyamide at 270°C in Dry Air

This table contains time-resolved rheometry measurements of a cyclo-aliphatic polyamide melt at 270°C under an oxidative dry air environment. Each row represents a measurement step recording viscoelastic properties, including storage and loss moduli and complex viscosity, over a period of two hours. The data tracks the influence of edge oxidation on the polymer melt's structural changes.

This table is useful for studying the kinetics of thermo-oxidative degradation and the resulting changes in viscoelasticity of polyamides. It provides raw experimental data for modeling edge gelation effects. It does not contain data for nitrogen environments or other temperatures (260°C or 275°C).

760 rows · 9 columns · published by Materials Cloud · licence: Open use, source must be named

Source file: https://archive.materialscloud.org/api/records/y12y2-j2z84/files/TPA_270C_Dry_Air_10rad.c… · the dataset

Columns

ColumnTypeDescription
Step TimeFLOATThe time elapsed since the start of the measurement step.
Oscillation StrainFLOATThe applied strain amplitude during oscillation.
Oscillation StressFLOATThe measured stress response during oscillation.
Tan DeltaFLOATThe ratio of loss modulus to storage modulus.
Storage ModulusFLOATThe measure of elastic energy stored in the material.
Loss ModulusFLOATThe measure of energy dissipated as heat.
Complex ViscosityFLOATThe overall resistance of the melt to flow.
Oscillation TorqueFLOATThe torque measured during the oscillation cycle.
GapFLOATThe distance between the parallel plates of the rheometer.

Questions it answers

Query it in SQL · API · Use it from an AI agent (MCP) · More tables